This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.
This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.
https://www.printables.com/model/129367-temperature-tower-ready-gcodes-abs-tpu-pla-asa-pet/files https://www.thingiverse.com/thing:3912855/files
I would suggest running the PLA temp tower and then you can optimize for that specific reel of filament.
I printed a tower a few days ago and it looks good anywhere from 200 to 215. I’m going to keep trying though.
You should also check your z offset and make sure that you’re not too close to the bed it’s possible that your nozzle is dragging because you’re less than .2 mm.