Hey everyone.
I built an mk3s+ from its kit form successfully, tested a few PLA prints with the stock 0.4 nozzle.
I’ve set prusaslicer to use a 0.6 nozzle now that I’ve upgraded, and am using PETG. Prints look pretty bad, in spite of calibrating z-offset etc.
If you were doing something like this for the first time, what would your setup steps be like?
To be specific, using a diamondback 0.6 nozzle, matterhackers PETG at 235c.
Issues I’m seeing are a really bad loss of detail, lots of stringing, etc.
eta: added a photo of a moderately post-processed part. Notice how rough the top surface looks, there’s a disconnect between perimeter loops, etc.
Laying down more material to speed prints as well as increase strength.